Composition: core of extruded polystyrene (XPS) board, compliant with the PN-EN 13164: 2010 norm, reinforced with fiberglass mesh on both sides and covered with a special high-quality cement mortar enriched with modified synthetic resins.
Declared coefficient of thermal conduction -design value according to Z-23.15-1476: DIN 4108-1, 0.03
d = 6 mm: 0.029
d = 12 mm: 0.029
d = 20 mm: 0.029
d = 30 mm: 0.029
d = 50 mm: 0.029
Apparent core density: › 36 kg / m³
Compression stress at 10% relative strain: ›0.3 MPa
Water absorption:
- after 1 hour: ‹ 1 kg / m²
- after 24 hours: ‹ 1 kg / m²
Operating temperature range: -50 ° C / + 75 ° C
Reaction to fire class: E